Operators in a powdered metals production facility heard a hissing noise near one of the plant furnaces and determined that it was a gas leak in the trench below the furnaces. The trench carried hydrogen, nitrogen, and cooling water runoff pipes as well as a vent pipe for the furnaces.

Maintenance personnel presumed that the leak was nonflammable nitrogen because there had recently been a nitrogen piping leak elsewhere in the plant. Using the plant's overhead crane, they removed some of the heavy trench covers. They determined that the leak was in an area that the crane could not reach, so they brought in a forklift with a chain to remove the trench covers in that area.

Eyewitnesses stated that as the first trench cover was wrenched from its position by the forklift view more

The incident occurred in the catalytic hydrotreatment plant of an oil refinery. The plant, which began operations in September 1997, has a capacity of 1650 tons/day of light fuel oil and 1450 tons/day of heavy fuel oil. The plant was designed to desulfurize the light and heavy fuel oil fractions produced in the refinery by treating them with high-pressure hydrogen over a catalyst to remove sulfur (producing hydrogen sulfide as a byproduct). The plant has two heating/reaction/fractionating sections to treat the two fuel oil fractions, but a single gas purification and compression section for the recycled hydrogen gas.

The heavy fuel oil reactor feedstock from the vacuum distillation plant is sent to the heavy fuel oil treatment section through three pipelines equipped with flow view more

An offgas system mishap involved two explosions occurring within an interval of about 3 ½ hours. The first offgas explosion was reportedly caused by a welding operation on an air line adjacent to a hydrogen sensor line containing off gas. The welding arc initiated a detonation within the offgas piping. The detonation was contained by the piping system but blew out the water seal at the base of the vent stack.The second hydrogen explosion in this incident occurred in the stack base area. Hydrogen accumulated in the enclosed base area after the water seal had been blown in the first explosion. The stack base metal door was blown off its hinges from the second explosion, and the reinforced concrete stack was also damaged. A plant employee walking by the stack at the time of the explosion view more